Experiment of the effect of pellet strength on Fe yield on direct reduction kiln was carried out on φ800 mm model kiln in laboratory.
在实验室80 0 mm回转窑火力模型上进行了球团强度对直接还原回转窑产品铁收得率影响的试验研究。